BLACK

PETG 2.0

SUNLU · PETG · BLACK

6 colors

1.23 g/cm³ · ±0.02 mm · OFD 2026-08-25

Nozzle
235 °C
230°tune within range240°
Bed
78 °C
75°tune within range80°

Before you print

2 things to know about this spool
  • Dry it before you print

    It quietly soaks up moisture from the air, which leaves prints rough, weak and stringy. Dry it at 65°C for about 4-6 hours first, then keep it sealed.

    65 °C~4-6 h
  • Print inside an enclosure

    It cools too fast in open air and can warp or crack. A closed-in printer holds the heat around the print (chamber at least 0°C).

New here? Nozzle = printing temperature in your slicer, bed = build plate. Start at the big number.
  • Nozzle is the hot-end temperature: enter it as the printing temperature in your slicer. Start at the big number; the range is the safe window to tune within.
  • Bed is the heated build plate: your slicer calls it bed temperature. It helps prints stick.
  • OFD is the Open Filament Database, the community-maintained database this catalog is built on.