PVA

PVA

ROSA3D Filaments · PVA

1.23 g/cm³ · ±0.02 mm · OFD 2026-08-25

Nozzle
195 °C
180°tune within range210°
Bed
55 °C
50°tune within range60°

Before you print

1 thing to know about this spool
  • Dry it before you print

    It quietly soaks up moisture from the air, which leaves prints rough, weak and stringy. Dry it at 40-45°C for about 4-6 hours first, then keep it sealed.

    40-45 °C~4-6 h