Nozzle
195 °C
180°tune within range210°
Bed
55 °C
50°tune within range60°
Before you print
1 thing to know about this spoolDry it before you print
It quietly soaks up moisture from the air, which leaves prints rough, weak and stringy. Dry it at 40-45°C for about 4-6 hours first, then keep it sealed.
40-45 °C~4-6 h
New here? Nozzle = printing temperature in your slicer, bed = build plate. Start at the big number.
- Nozzle is the hot-end temperature: enter it as the printing temperature in your slicer. Start at the big number; the range is the safe window to tune within.
- Bed is the heated build plate: your slicer calls it bed temperature. It helps prints stick.
- OFD is the Open Filament Database, the community-maintained database this catalog is built on.
Specs
- Diameter
- 1.75 mm
- Spool sizes
- 500 g
- Density
- 1.27 g/cm³
- Diameter tolerance
- ±0.03 mm
Available colors (1)
Clear
#F0F1A8
Sources & verification
- Data: Open Filament Database
- Manufacturer datasheet: https://cdn.shopify.com/s/files/1/0651/1555/4032/files/Bambu_PVA_Technical_Data_Sheet.pdf?v=1715140818
- Safety datasheet: https://cdn.shopify.com/s/files/1/0584/7236/6216/files/MSDS_Bambu_PVA.pdf?v=1710243141
- OFD snapshot generated: 2026-08-25