Nozzle
225 °C
210°tune within range240°
Bed
43 °C
25°tune within range60°
Before you print
1 thing to know about this spoolDry it before you print
It quietly soaks up moisture from the air, which leaves prints rough, weak and stringy. Dry it at 50-60°C for about 6-12 hours first, then keep it sealed.
50-60 °C~6-12 h
New here? Nozzle = printing temperature in your slicer, bed = build plate. Start at the big number.
- Nozzle is the hot-end temperature: enter it as the printing temperature in your slicer. Start at the big number; the range is the safe window to tune within.
- Bed is the heated build plate: your slicer calls it bed temperature. It helps prints stick.
- OFD is the Open Filament Database, the community-maintained database this catalog is built on.
Specs
- Diameter
- 1.75 mm
- Spool sizes
- 1 kg
- Density
- 1.12 g/cm³
- Diameter tolerance
- ±0.05 mm
- Shore A
- 90
Available colors (3)
Black
#16161A
Sources & verification
- Data: Open Filament Database
- Temperatures: Snapmaker TPU 90A Technical Data Sheet V1.0.0
- OFD snapshot generated: 2026-08-25
Related spools
same family, popular brands firstSnapmakerTPU
High Flow TPU95
210°C nozzle temperature
SnapmakerTPU
TPU
220°C nozzle temperature
SnapmakerTPU
TPU 95A HF
225°C nozzle temperature
eSUN 3DTPU
TPU-95APick
The most beginner-friendly TPU: 95A shore hardness strikes the balance between flexibility and printability.
225°C nozzle temperature
OvertureTPU
TPUPick
The classic first flexible: forgiving 95A shore, prints on stock Bowden printers if you go slow.
225°C nozzle temperature
Bambu LabTPU
TPU
225°C nozzle temperature