Nozzle
275 °C
265°tune within range285°
Bed
110 °C
100°tune within range120°
Before you print
2 things to know about this spoolDry it before you print
It quietly soaks up moisture from the air, which leaves prints rough, weak and stringy. Dry it at 80-90°C for about 6-8 hours first, then keep it sealed.
80-90 °C~6-8 hPrint inside an enclosure
It cools too fast in open air and can warp or crack. A closed-in printer holds the heat around the print.
New here? Nozzle = printing temperature in your slicer, bed = build plate. Start at the big number.
- Nozzle is the hot-end temperature: enter it as the printing temperature in your slicer. Start at the big number; the range is the safe window to tune within.
- Bed is the heated build plate: your slicer calls it bed temperature. It helps prints stick.
- OFD is the Open Filament Database, the community-maintained database this catalog is built on.
Specs
- Diameter
- 1.75 mm
- Spool sizes
- 970 g
- Density
- 1.22 g/cm³
- Diameter tolerance
- ±0.03 mm
Available colors (5)
Jet Black
#24292A
Editorial notesUpdated 2026-07-10
The most approachable polycarbonate: Prusa blended it to print without an industrial machine. You still want an enclosure and a well-dried spool.
Sources & verification
- Data: Open Filament Database
- Temperatures: Prusament (prusament.com)
- OFD snapshot generated: 2026-08-25