Black

TPU

Professional LAB · TPU · Black

8 colors

1.25 g/cm³ · ±0.03 mm · OFD 2026-08-25

Nozzle
220 °C
205°tune within range235°
Bed
55 °C
50°tune within range60°

Before you print

1 thing to know about this spool
  • Dry it before you print

    It quietly soaks up moisture from the air, which leaves prints rough, weak and stringy. Dry it at 50°C for about 6-12 hours first, then keep it sealed.

    50 °C~6-12 h
New here? Nozzle = printing temperature in your slicer, bed = build plate. Start at the big number.
  • Nozzle is the hot-end temperature: enter it as the printing temperature in your slicer. Start at the big number; the range is the safe window to tune within.
  • Bed is the heated build plate: your slicer calls it bed temperature. It helps prints stick.
  • OFD is the Open Filament Database, the community-maintained database this catalog is built on.