PC-FR

PC-FR

ELEGOO · PC

1.18 g/cm³ · ±0.02 mm · OFD 2026-08-25

Nozzle
270 °C
260°tune within range280°
Bed
100 °C
90°tune within range110°

Before you print

2 things to know about this spool
  • Dry it before you print

    It quietly soaks up moisture from the air, which leaves prints rough, weak and stringy. Dry it at 85°C for about 6-8 hours first, then keep it sealed.

    85 °C~6-8 h
  • Print inside an enclosure

    It cools too fast in open air and can warp or crack. A closed-in printer holds the heat around the print (chamber at least 45°C).

New here? Nozzle = printing temperature in your slicer, bed = build plate. Start at the big number.
  • Nozzle is the hot-end temperature: enter it as the printing temperature in your slicer. Start at the big number; the range is the safe window to tune within.
  • Bed is the heated build plate: your slicer calls it bed temperature. It helps prints stick.