Nozzle
230 °C
Bed
60 °C
Before you print
1 thing to know about this spoolDry it before you print
It quietly soaks up moisture from the air, which leaves prints rough, weak and stringy. Dry it at 50-60°C for about 6-12 hours first, then keep it sealed.
50-60 °C~6-12 h
New here? Nozzle = printing temperature in your slicer, bed = build plate. Start at the big number.
- Nozzle is the hot-end temperature: enter it as the printing temperature in your slicer. Start at the big number; the range is the safe window to tune within.
- Bed is the heated build plate: your slicer calls it bed temperature. It helps prints stick.
- OFD is the Open Filament Database, the community-maintained database this catalog is built on.
Specs
- Diameter
- 1.75 mm
- Spool sizes
- 300 g
- Density
- 1.2 g/cm³
- Diameter tolerance
- ±0.02 mm
Available colors (10)
Black 85A
#000000
Sources & verification
- Data: Open Filament Database
- Temperatures: SpoolmanDB
- OFD snapshot generated: 2026-08-25
Related spools
same family, popular brands firstAzureFilmTPU
TPU 85A
230°C nozzle temperature
eSUN 3DTPU
TPU-95APick
The most beginner-friendly TPU: 95A shore hardness strikes the balance between flexibility and printability.
225°C nozzle temperature
OvertureTPU
TPUPick
The classic first flexible: forgiving 95A shore, prints on stock Bowden printers if you go slow.
225°C nozzle temperature
Bambu LabTPU
TPU
225°C nozzle temperature
Bambu LabTPU
TPU 85A
225°C nozzle temperature
HatchboxTPU
TPU
225°C nozzle temperature