Black

PA12 Adura

Add-North · PA12 · Black

5 colors

1.1 g/cm³ · ±0.02 mm · OFD 2026-08-25

Nozzle
258 °C
245°tune within range270°
Bed
68 °C
60°tune within range75°

Before you print

2 things to know about this spool
  • Dry it before you print

    It quietly soaks up moisture from the air, which leaves prints rough, weak and stringy. Dry it at 70°C for about 12-16 hours first, then keep it sealed.

    70 °C~12-16 h
  • Print inside an enclosure

    It cools too fast in open air and can warp or crack. A closed-in printer holds the heat around the print.

New here? Nozzle = printing temperature in your slicer, bed = build plate. Start at the big number.
  • Nozzle is the hot-end temperature: enter it as the printing temperature in your slicer. Start at the big number; the range is the safe window to tune within.
  • Bed is the heated build plate: your slicer calls it bed temperature. It helps prints stick.
  • OFD is the Open Filament Database, the community-maintained database this catalog is built on.