Nozzle
275 °C
260°tune within range290°
Bed
80 °C
Before you print
2 things to know about this spoolDry it before you print
It quietly soaks up moisture from the air, which leaves prints rough, weak and stringy. Dry it at 70-90°C for about 12-16 hours first, then keep it sealed.
70-90 °C~12-16 hPrint inside an enclosure
It cools too fast in open air and can warp or crack. A closed-in printer holds the heat around the print.
New here? Nozzle = printing temperature in your slicer, bed = build plate. Start at the big number.
- Nozzle is the hot-end temperature: enter it as the printing temperature in your slicer. Start at the big number; the range is the safe window to tune within.
- Bed is the heated build plate: your slicer calls it bed temperature. It helps prints stick.
- OFD is the Open Filament Database, the community-maintained database this catalog is built on.
Specs
- Diameter
- 1.75 mm
- Spool sizes
- 1 kg
- Density
- 1.01 g/cm³
- Diameter tolerance
- ±0.02 mm
Available colors (1)
Natural
#E4E1D0
Sources & verification
- Data: Open Filament Database
- Temperatures: Spectrum PA6 GK10 TDS (spectrumfilaments.com)