Nozzle
265 °C
250°tune within range280°
Bed
95 °C
80°tune within range110°
Before you print
2 things to know about this spoolDry it before you print
It quietly soaks up moisture from the air, which leaves prints rough, weak and stringy. Dry it at 70-90°C for about 12-16 hours first, then keep it sealed.
70-90 °C~12-16 hPrint inside an enclosure
It cools too fast in open air and can warp or crack. A closed-in printer holds the heat around the print.
Manufacturer didn't publish exact temps for this filament. The numbers above are the typical PA6 range. Confirm them on your first print.
New here? Nozzle = printing temperature in your slicer, bed = build plate. Start at the big number.
- Nozzle is the hot-end temperature: enter it as the printing temperature in your slicer. Start at the big number; the range is the safe window to tune within.
- Bed is the heated build plate: your slicer calls it bed temperature. It helps prints stick.
- OFD is the Open Filament Database, the community-maintained database this catalog is built on.
Specs
- Density
- 1.24 g/cm³
- Diameter tolerance
- ±0.02 mm
Sources & verification
- Data: Open Filament Database
- OFD snapshot generated: 2026-10-17